This article outlines Volkswagen's strict guidelines regarding the use of heat during structural and panel repairs. Volkswagen prohibits heating high-strength and ultra-high-strength steel during reforming, restricts heat use on mild steel due to degradation of material strength and corrosion resistance, and only permits controlled heating up to 150°C (302°F) on aluminum panels using thermo-strips for temperature monitoring.

What to do on the job

Do not apply heat when straightening high-strength or ultra-high-strength steel, and limit heat on aluminum panels to a maximum of 150°C (302°F) monitored strictly with thermo-strips.

How to use it

Use this document to justify the replacement of high-strength steel structural components that cannot be cold-straightened, and to support line items for thermo-strips and temperature monitoring equipment when performing aluminum dent repairs.

Read the original at I-CAR ↗

This page is a summary written by TechnicianVision. The document itself belongs to its publisher — follow the link above to read it in full.

TechnicianVision puts procedures like this next to the repair order you are working on. Create a free account →