TechnicianVision · Knowledge base

Straightening And Heat: Rivian

I-CAR · February 13, 2025 · Rivian

Summary

This article outlines Rivian's guidelines on using heat for straightening structural and cosmetic components, referencing model-specific Material Matrices. For conventional steel, Rivian permits heat straightening only for minor panel damage, with a strict limit of two heating cycles and a maximum temperature of 600°C (1,112°F).

What to do on the job

Consult the model-specific Rivian Material Matrix before applying heat, and ensure conventional steel is heated no more than twice and never exceeds 600°C (1,112°F).

How to use it

Use this document to justify the time and equipment (such as temperature-monitoring tools) required to safely perform controlled heating on Rivian vehicles, or to support the replacement of a component if the Material Matrix prohibits heat straightening for that specific metal type.

Read the original at I-CAR ↗

This page is a summary written by TechnicianVision. The document itself belongs to its publisher — follow the link above to read it in full.

TechnicianVision puts procedures like this next to the repair order you are working on. Create a free account →